一.適用:
棉布,化纖布,毛衣、毛巾或其它高要求無(wú)手感的織布涂料印花,印在面料上手感超軟。
二.特性
本品是一種新技術(shù)、新突破反應(yīng)性基因的高分子共聚粘合劑,屬陰離子型,在織物上可起到交聯(lián)及自交聯(lián)作用。
由于本產(chǎn)品具有無(wú)手感特性,用本產(chǎn)品印出來(lái)的產(chǎn)品手感與染料印花手感一模一樣,因此用涂料印花代替染料印花變?yōu)榭赡。手搓輕微泛白,水洗后手感超柔軟,干濕擦牢度好,干濕擦達(dá)到3-4級(jí),摩擦痕跡不明顯,本品不含甲醛,不含壬基苯酚,不含鄰苯二甲酸酯,因此是織物印花最理想的無(wú)毒性環(huán)保產(chǎn)品。
三.外觀組成及說(shuō)明:
序號(hào) |
項(xiàng) 目 |
指 標(biāo) |
1 |
外觀 |
乳白色乳液 |
2 |
固含量(%) |
45±1 |
3 |
PH值 |
6~8 |
故障與排除:
1、牢固度欠佳大概有以下幾種可能性造成:
1、布料不是綿布,布面比較光滑,或布面殘留柔軟硅油太多
指引:增加CH-701仿活性固漿的份量,或添加1~1.5%催化劑可以將牢固度提升1~2倍.
2、天氣潮濕,漿面沒有充分干透
指引:150度烘1~2分鐘或150度壓燙10~15秒,一般要完全干透24小時(shí)后才能達(dá)到最佳洗水牢度。
3、色漿加量超10%以上
指引:選用濃度更高的色漿即可降低色漿的使用比例。
Other detailed information
Brand |
Conghui |
Model |
CH701 |
Viscosity |
/ |
PH value |
/ |
Odor |
/ |
Strength |
T |
Fineness |
/um |
Appearance |
|
Usage |
|
Color strength |
100% |
Fluidity |
/mm |
Shelf life |
12months |
Single net weight |
50KG |
Resin type |
/ |
Ionic |
/ |
Appearance color |
|
一.Substrates :
Cotton ,chemical fabric,sweater,towel or other high requirement,no hand feeling fabric pigment printing, print on the fabric with soft hand feel.
二.Features
This product is a new technological,new breakthrough reactive polymer adhesive, belongs to anion,it can reach the effect of crosslinking or self-crosslinking on fabric.
Due to this product with a feature of no hand feeling, the effect of product which used this product to print can be same as pigment printing.so that use pigment printing instead of dye printing has been a possibility.It becomes slightly white after hand rubbing,super soft hand feel after washing,excellent performance of wet and dry rub,it can reach 3-4 degree,The marks of friction are not obvious.
This product no contains formaldehyde,nonylphenol and phthalate, so that this product is the most ideal non-toxic environmental product.
三.Appearance composition and specification
Sequence number |
project |
Indicator |
1 |
Appearance |
Ivory emulsion |
2 |
Solid content |
45±1 |
3 |
PH value |
6~8 |
Troubles and elimination:
1.The ability of fastness do not well could be caused by several possibilities as follow:
1.The fabric is not cotton, the surface is smooth or the surface exists too much soft silicone oil.
Guidance: increase the amount of CH-701 reactive paste or add 1~1.5% catalyst could improve the ability of fastness one or two times.
2.In wet weather, the surface of paste without dry completely.
Guidance:Baking 1~2 minutes at 150℃ or heat pressure10~15secondsat 150℃,it could reach the best ability of wash after drying 24hours.
3.The amount of pigment paste more than 10%
Guidance:adopting higher concentration pigment paste so that it can reduce the rate of pigment paste.